19174
Accession Number
37968
Title Of Article Chaper
The repair of parchment: filling
Title Of Journal Book
Reviews in conservation
Issue
1
Pages
77-86
Reference Bibliography
53 bibliog. refs.
ISSN
1605-8410
Language Of Text
English
Language Of Summary
English
Literature Type
Serial
Literature Level
Analytic
Abstract
Parchment is produced by processing the deraml layer of animal hide through limited mechanical and chemical treatment and then drying it under tension. The weak condition of many historical objects made of this material is caused by chemical, biological and mechanical degradation. Repairing these objects by filling gaps with parchmet or paper patches may be inadvisable, due to important differences in intrinsic strength, which can create tensions between old and new materials. Alternative filling methods may be used, consisting of the application of solid materials in the form of a powder or a suspension, used to create a solid sheet of reconstituted parchment. The solids may consist of any kind of collagenous material (powdered parchment or hide, gelatin), paper or a comnbination of the two. Published methods describe preliminary treatments (e.g. relaxation), application media (water, solvents, additives), use of additional consolidating membrane (Japanese paper, goldbeaters's skin), use of adhesives for pasting and surface consolidation purposes, preparation of mechanically isotropic templates for infills and tinting with synthetic dyes. A comparative investigation of methods confirms that the mechanical properties achieved in these infills, such as tensile strength and elasticity, as well as their reproducibility, are acceptable for application in conservation practice.
Keywords
Parchment; Restoration; Lacuna; Reintegration; Repair; Leafcasting; Bibliography